TA Instruments Differential Scanning Calorimeter (DSC-2920)
Features and Specifications:
- Maximum sample size is diameter or side 4 mm, thickness 1 to 2 mm, mass max 300 mg
- Temperature range is -75°C to 400°C
- Heating rates are between 0.1°C/min and 30°C/min
- Crucibles of aluminium and copper
- Indirect resistance heating
- Inert (argon, helium, nitrogen) atmosphere
Typical Applications:
- Studying thermal transitions of solids and liquids
- Thermal characterization of polymers, such as glass transition temperature, crystallization temperature and metling point